Polycarbonate (PC): Properties, Grades, and Injection Molding Guide
Need Custom Components?
Looking for a direct China factory for plastic or hardware parts?
Your Direct China Manufacturer
In-house production for custom plastic and hardware parts.
What Determines the Result of a Polycarbonate Part?
The most counterintuitive fact about polycarbonate is that high impact strength does not make it resistant to every form of damage. PC plastic can absorb severe impact, yet it may scratch more easily than expected, develop stress cracking after contact with certain chemicals, or become brittle when it has been processed with excessive moisture and internal stress.

For a molded PC component, three variables normally determine the final result. They should be reviewed in this order because each one sets the conditions for the next:
- Material grade and additives: The selected grade controls impact performance, heat resistance, transparency, UV stability, flame behavior, color, and processing range.
- Moisture and thermal history: Poor drying or excessive residence time can reduce molecular weight and create visible or hidden quality problems.
- Part geometry and tooling: Wall thickness, gates, ribs, corners, vents, and cooling balance determine whether the selected PC material can fill and release reliably.
Material grade has the highest priority because a standard transparent grade cannot be expected to perform like a UV-stabilized, flame-retardant, or glass-reinforced grade. Moisture and heat then determine whether the resin retains its designed properties during PC injection molding. Geometry and tooling convert those material and process decisions into actual dimensions, appearance, and service life.
Polycarbonate Material: Core Properties and Practical Limits
Polycarbonate is an amorphous engineering thermoplastic known for high impact resistance, good dimensional stability, transparency, and useful heat resistance. It is used for structural housings, covers, guards, brackets, electrical components, tool accessories, and other general plastic parts where ordinary commodity plastics may not provide enough toughness.
However, PC material is not automatically the best choice whenever strength is required. Its performance depends on load duration, temperature, notch shape, chemical exposure, surface finish, and the quality of molding. A purchasing specification should therefore describe the working conditions rather than simply requesting “polycarbonate.”
| Polycarbonate property | What it means for part selection | Manufacturing implication |
|---|---|---|
| High impact toughness | Suitable for parts exposed to drops, knocks, or intermittent mechanical shock. | Sharp corners, thin sections, weld lines, and poorly molded notches can reduce real-world toughness. |
| Good transparency in suitable grades | Useful when visibility or light transmission is required. | Drying, clean handling, polished tooling, and controlled filling are important for optical appearance. |
| Relatively high heat resistance | More suitable than many general-purpose plastics for elevated-temperature service. | Actual continuous-use performance depends on grade, load, duration, and surrounding environment. |
| Moisture sensitivity during processing | Resin may look acceptable while still containing enough moisture to affect quality. | Drying conditions, hopper control, storage, and material traceability require attention. |
| Limited resistance to some chemicals | Contact with solvents, alkaline cleaners, oils, or other chemicals must be reviewed. | Stress, sharp features, and chemical exposure can combine to cause cracking. |
| Moderate scratch resistance | Clear or visible surfaces may show handling marks during assembly or use. | Surface texture, protective films, packaging, and handling procedures can affect acceptance. |
| UV performance varies by grade | Outdoor use requires suitable stabilization or a protective design. | A general-purpose indoor grade should not be specified for long-term sunlight exposure without validation. |
Impact Strength Does Not Mean Unlimited Durability

PC plastic generally performs well under impact, but impact resistance is reduced by notches, sharp internal corners, holes close to edges, weld lines, and excessive residual stress. A part that passes a simple drop test may still crack after assembly if a screw boss is over-tightened or if a press-fit creates high local stress.
For this reason, the drawing should show generous radii at load-bearing transitions. Bosses and clips should be designed so that assembly force is distributed rather than concentrated at a thin root. When a component must remain tough at low temperature, testing should be performed at the expected service temperature instead of only at room temperature.
Transparency, Surface Finish, and Scratching
Transparent polycarbonate is often selected for its appearance, but a clear part exposes more process variation than an opaque part. Flow marks, weld lines, black specks, silver streaks, small bubbles, and uneven gloss can become immediately visible. A polished mold surface alone cannot correct poor resin drying or unstable filling.
PC is also less scratch-resistant than glass and some specialty optical materials. If a clear cover will be wiped frequently, exposed to abrasive dust, or handled during assembly, the specification should address allowable surface marks, protective packaging, and any required coating or secondary treatment. These requirements can affect tooling, cycle time, cost, and inspection criteria.
Heat, Chemical, and Outdoor Considerations
Polycarbonate retains useful mechanical performance at temperatures where many standard plastics soften, but the actual limit is grade-specific. A part under constant load may deform at a temperature below the material’s short-term heat rating. Engineers should review the load, duration, mounting method, and temperature cycle together.
Chemical compatibility is another frequent source of field failure. Certain solvents, cleaning agents, fuels, oils, adhesives, and alkaline substances can cause environmental stress cracking, especially when the part is already under tensile stress. A PC component used near chemicals should be tested with the actual substance and exposure duration. A general statement such as “chemical resistant” is not sufficient for supplier approval.
For outdoor applications, UV-stabilized PC or a suitable protective design may be required. Colorants and additives can also affect weathering, appearance, and mechanical properties. If the part is exposed to sunlight, specify the expected exposure and acceptance criteria instead of relying only on the basic resin name.
How to Select the Right PC Plastic Grade
Grade selection should begin with the part’s environment and function. The lowest-cost standard grade may be appropriate for an indoor housing, while a visible outdoor cover or a component near a heat source may require a different formulation. A material datasheet should be reviewed together with the part drawing and intended use.
- General-purpose PC: Suitable for many structural and functional components where impact strength and dimensional stability are important.
- UV-stabilized PC: Consider when the component will receive prolonged sunlight or outdoor exposure.
- Flame-retardant PC: Consider only when the application requires a defined flame behavior and the selected grade has the required test documentation.
- Glass-reinforced PC: May improve stiffness and reduce some forms of deformation, but can increase anisotropy, warpage risk, visible fiber effects, and tooling wear.
- Optical or appearance-focused PC: Requires tighter control of resin cleanliness, drying, tooling finish, filling, and handling.
- PC blends such as PC/ABS: May offer a different balance of processability, toughness, appearance, and cost. They should not be treated as identical to unmodified PC.
When requesting quotations, buyers should identify the resin family, preferred grade or approved equivalent, color, gloss or texture, transparency requirement, operating temperature, chemical exposure, and any testing requirement. If the grade is not fixed, the supplier should state the proposed material clearly so that a cost comparison does not hide a performance difference.
Polycarbonate Compared with Other Common Plastics
PC material is often compared with ABS, PMMA, and other engineering plastics. The correct choice depends on the dominant requirement rather than on a single headline property.
- PC versus ABS: PC generally provides higher impact toughness and heat capability, while ABS may offer easier processing, a wider economical range, and good surface appearance for many indoor housings. If the part is frequently dropped or exposed to higher heat, PC may be justified. If cost and easy cosmetic molding dominate, ABS may be more practical.
- PC versus PMMA: PMMA is often selected for excellent optical clarity, surface hardness, and weathering characteristics in suitable grades. PC is generally preferred where impact toughness is more important. A transparent part that must resist impact should not be specified as PMMA solely because it looks clear in a sample.
- PC versus POM: POM is commonly considered for low-friction, wear-related, or sliding functions, while PC is more suitable for transparent, impact-resistant, and structurally visible components. The two materials should not be substituted without reviewing friction, chemical exposure, and dimensional requirements.
- PC versus reinforced materials: Reinforcement can increase stiffness but may make the part more directionally dependent and more difficult to mold cosmetically. The benefit should be confirmed against the actual load case.
For general components and hardware-related plastic parts, the practical decision is often a balance between impact performance, appearance, chemical exposure, tooling complexity, and unit cost. A supplier should be able to explain what changes when the material is downgraded, blended, colored, or reinforced.
PC Injection Molding: Process Requirements
PC injection molding is reliable when moisture, temperature, filling, cooling, and part design are controlled together. Polycarbonate usually requires more process discipline than commodity plastics because excessive moisture and thermal stress can quickly affect appearance and mechanical performance.
Drying and Material Handling
Polycarbonate is hygroscopic enough to require thorough drying before molding. Moisture can react with the polymer during processing and cause hydrolysis. Typical drying practice for many PC grades may involve approximately 100 to 120°C for several hours, with a moisture target often specified below 0.02 percent. These are starting references only; the resin supplier’s datasheet and the actual dryer performance should control the process.
Drying time alone does not guarantee dry resin. Open bags, humid storage, an overloaded hopper, poor air flow, or long transfer lines can allow the material to absorb moisture again. A controlled process should address sealed storage, lot identification, drying records, and the maximum permitted time between drying and molding.
Melt Temperature, Mold Temperature, and Filling
Many PC grades are processed at a relatively high melt temperature, often within an approximate range of 280 to 320°C. Mold temperatures commonly require a higher setting than standard commodity plastics, frequently around 80 to 120°C depending on grade, wall thickness, appearance, and cycle requirements. The correct values must come from the material supplier and be confirmed through sampling.
A higher mold temperature can improve flow, reduce visible weld lines, and lower residual stress, but it may increase cycle time. Excessive melt temperature or long residence time can cause discoloration, degradation, or black specks. The molding team should avoid using heat as the only solution for a poorly designed gate or an overly thin wall.
Filling should be stable rather than unnecessarily aggressive. Injection speed may need to change through the fill to control shear, jetting, and weld-line appearance. Adequate venting is important because trapped air can cause burns, short shots, or local cosmetic defects.
Part and Mold Design for PC Components
Uniform wall thickness is one of the most effective ways to reduce shrinkage variation and internal stress. Sudden transitions, heavy bosses, thick ribs, and isolated material accumulations can create sink marks or uneven cooling. Where a thick feature is necessary, coring and gradual transitions should be considered.
- Use rounded transitions: Internal radii reduce stress concentration and improve melt flow around corners.
- Keep ribs and bosses proportionate: As a starting design practice, ribs are often kept near 40 to 60 percent of the adjoining nominal wall thickness, with the final value confirmed through molding trials.
- Provide suitable draft: A draft angle of about 0.5 to 1 degree per side may be a starting point, but textured surfaces and deep features often require more.
- Place gates thoughtfully: Gate position affects weld lines, visible flow marks, packing, fiber orientation in reinforced grades, and dimensional stability.
- Vent the mold effectively: Venting near the end of fill and around difficult features helps prevent trapped-air burns and incomplete filling.
- Control cooling balance: Uneven mold temperatures or cooling channels can produce warpage even when the material and dimensions appear correct.
For transparent or high-gloss parts, the gate, ejector marks, parting line, and flow direction should be reviewed before mold construction. A drawing that defines only dimensions but not visible surfaces can lead to disagreement during sample approval.
Common PC Injection Molding Defects and Their Causes
Splay, Silver Streaks, and Bubbles
Silver streaks or splay are commonly associated with moisture, trapped gas, excessive shear, or poor material handling. If the defect follows the flow direction and appears as a fine, shiny streak, drying and venting should be checked before changing the color or polishing the tool. Bubbles may also result from gas entrapment, insufficient packing, or local thick sections.
Weld Lines and Brittle Areas
Weld lines form where separate flow fronts meet. They are not automatically unacceptable, but they can reduce appearance and local strength. Their position should be kept away from impact zones, snap-fit roots, and highly stressed openings when possible. Raising mold temperature, improving venting, changing gate location, or adjusting filling speed may help, but the best solution may be a tool or geometry change.
Warpage, Sink, and Dimensional Variation
Warpage is usually connected to uneven shrinkage, inconsistent cooling, unbalanced filling, or directional reinforcement. Sink marks often appear around thick bosses and ribs. Measuring only a flat dimension after molding may not reveal the cause. The inspection plan should include critical datums, flatness or runout where relevant, assembly fit, and dimensions after conditioning if the application requires it.
Stress Cracking and Assembly Damage
Stress cracking may occur after molding rather than immediately at the machine. Common contributors include excessive clamp force from screws, tight press-fits, aggressive cleaning agents, sharp corners, and residual molding stress. When a PC component is assembled with hardware, torque limits and assembly sequence should be validated rather than left to operator judgment.
Quality Control and Validation for PC Parts
A practical validation plan should connect material, process, dimensions, appearance, and intended use. The exact tests depend on the component, but a supplier evaluation normally benefits from the following checkpoints:
- Confirm the resin grade, color, lot information, and applicable material documentation.
- Verify drying records and establish how opened material is stored and reused.
- Inspect critical dimensions against the approved drawing and reference datums.
- Define acceptable limits for weld lines, flow marks, black specks, scratches, sink, flash, and gate marks.
- Check assembly fit, screw torque, clip function, or insertion force where the part will be assembled with hardware.
- Perform drop, impact, heat, chemical, UV, or aging tests when those conditions are relevant to service.
- Approve a representative production sample rather than evaluating only a hand-finished prototype.
For transparent PC parts, appearance inspection should be performed under an agreed lighting condition and viewing distance. For functional structural parts, cosmetic approval alone is not enough; dimensions, assembly stress, and environmental exposure may be more important than surface gloss.
Purchasing and Supplier Coordination for PC Injection Molding
A clear RFQ reduces both quotation differences and later engineering changes. The package should include the 3D model, 2D drawing, expected annual or batch volume, material requirement, color standard, visible-surface definition, critical tolerances, assembly information, and delivery expectations. If the mold will be used for long-term production, the quotation should also clarify trial samples, changes after approval, spare parts, maintenance responsibility, and ownership terms.
Buyers should pay particular attention to substitutions. “PC equivalent” can refer to materials with different impact strength, melt flow, flame behavior, UV performance, or color stability. Any alternative grade should be approved against the functional requirements rather than accepted only because the basic polymer name is similar.
JATERSON is a Zhejiang-based manufacturing company focused on injection molding and hardware production. For PC component projects, our relevant support covers engineering review, sample development, mold-related coordination, production ramp-up, quality control, lead-time management, and OEM or ODM project communication. The practical objective is to connect material selection with manufacturable geometry, stable molding, inspection requirements, and repeatable delivery.
Polycarbonate is a strong material choice when impact resistance, heat performance, and design flexibility are important. It becomes a risky choice when moisture control, chemical exposure, surface requirements, or internal stress are ignored. The most reliable results come from approving the grade, part design, molding conditions, and inspection standard as one connected manufacturing decision.