Send a drawing, 3D file or sample of your plastic component.
Custom plastic injection molding, with supporting hardware parts reviewed per project.
Water Absorption Problems Often Start After Sample Approval
A molded plastic component passes dimensional inspection, but the same part becomes tight around a metal pin after storage in a humid warehouse. Another batch looks acceptable but develops brittle failures because the resin entered the molding machine with excessive moisture. Both problems involve water, but they occur at different stages and require different controls.

The common mistake is treating water absorption as a single datasheet number rather than a condition that affects material selection, molding, inspection, and service performance. A part measured shortly after molding may not represent the condition in which an overseas customer assembles or uses it.
JATERSON is a Zhejiang-based manufacturer with more than 20 years of production experience in plastic injection molding and hardware manufacturing. For general plastic components, tool accessories, and related OEM/ODM work, the practical question is not simply whether a polymer absorbs water. It is whether that absorption changes the part enough to affect fit, function, quality, or delivery.
The safest approach is to define the service environment, select the exact resin grade, control pellet moisture, and approve parts in an agreed moisture condition before releasing tooling and production requirements.
What Water Absorption Means for Plastic Components
Water absorption is the uptake of water into a material under specified exposure conditions. In plastics, it is commonly reported as a percentage increase in specimen mass relative to its initial dry mass.
Water absorption (%) = [(mass after exposure − initial dry mass) / initial dry mass] × 100.
For example, a specimen increasing from 10.000 g to 10.080 g has a measured mass gain of 0.80%. This calculation is meaningful only when the initial drying procedure, exposure conditions, surface-water removal, and weighing procedure are controlled. Material loss or extraction during immersion can also complicate interpretation.
Water immersion and atmospheric humidity are different exposures
A 24-hour water-immersion result does not describe equilibrium moisture content in an indoor assembly environment. Liquid-water exposure, humid air, temperature, wall thickness, and exposure duration all influence the result. Thin test specimens can approach equilibrium faster than thick molded sections.

Polymer moisture absorption also depends on chemistry. Polyamides contain polar groups that interact strongly with water, while polypropylene has much lower bulk water uptake under ordinary ambient conditions. Fillers, reinforcement, additives, and polymer blends change the behavior of a specific commercial grade.
Absorption is not the same as surface condensation
Water can remain on pellet surfaces without being absorbed deeply into the polymer. For example, cold pellets opened in a warm, humid molding area can collect condensation. Even a low-absorption resin may therefore need attention before processing.
Conversely, pellets that look dry can contain internal moisture. Visual inspection alone cannot establish whether a hygroscopic engineering resin is ready for molding.
Compare Water Absorption of Plastics by Application, Not Ranking Alone
A useful comparison begins with candidate material families, but purchasing approval must identify the actual manufacturer and grade. Unfilled, glass-fiber-reinforced, impact-modified, and flame-retardant versions should not be treated as interchangeable.
The table below provides screening guidance for molded mechanical components. It deliberately avoids universal absorption percentages: published values may use different specimen thicknesses, exposure periods, or conditioning methods.
| Material candidate | Moisture-related consideration | Potential manufacturing or functional consequence | Required selection check |
|---|---|---|---|
| PA6 and PA66, unfilled grades | Moisture uptake is important in ambient-humidity and immersion applications. | Conditioning can increase dimensions, reduce stiffness, and increase ductility compared with the dry state. | Compare dry and conditioned properties for the exact grade; validate critical fits after defined exposure. |
| Glass-fiber-reinforced PA6 or PA66 | Reinforcement changes composite uptake and constrains dimensional response unevenly. | Fiber orientation can make dimensional change direction-dependent. | Test the molded geometry and relevant directions, not only a standard specimen. |
| PA12 | Generally has lower moisture uptake than PA6 or PA66 under comparable conditions. | May offer better moisture-related dimensional consistency, but other mechanical properties differ. | Confirm stiffness, creep, temperature requirements, grade availability, and cost. |
| POM | Usually has lower moisture uptake than PA6 or PA66, but uptake is not zero. | Can be a candidate for moving parts and precision fits where its other properties are suitable. | Review immersion data, chemical exposure, load, and dimensional results for the selected grade. |
| PP and PE | Low bulk water absorption under ordinary ambient conditions. | Moisture stability alone does not ensure sufficient stiffness, creep resistance, or heat resistance. | Check load, temperature, shrinkage, and assembly tolerances before substitution. |
| PBT, PET, and PC | Service uptake and allowable moisture before melt processing are separate issues. | Excess pellet moisture can cause processing defects or molecular degradation at melt temperature. | Follow grade-specific drying and residual-moisture limits; verify molded-part performance separately. |
A lower absorption value does not automatically identify the better material. Replacing a polyamide bracket with polypropylene may reduce moisture-related swelling but introduce unacceptable creep or deflection. The decision must address the complete load, temperature, chemical, and tolerance requirements.
Read Test Results Before Comparing Supplier Datasheets
ASTM D570 and ISO 62
ASTM D570 and ISO 62 are commonly used to evaluate water absorption of plastics. Both provide controlled testing frameworks, but a standard reference by itself does not make two reported values directly comparable.
A result described as “24-hour water absorption” should not be compared directly with a saturation value or an atmospheric-humidity equilibrium value. Even within one standard, the selected procedure and specimen details matter. Ask for the test conditions behind the number.
- Exact resin manufacturer, grade designation, and reinforcement content.
- Test standard, applicable procedure, and specimen dimensions.
- Initial drying or conditioning procedure.
- Exposure medium, temperature, relative humidity where applicable, and duration.
- Whether the value represents a fixed exposure time or equilibrium.
- Surface-water removal and weighing procedure.
Conditioning and pellet moisture require different methods
ISO 291 provides standard atmospheres for conditioning and testing plastics. An agreed atmosphere such as 23°C and 50% relative humidity can make inspection conditions clearer, but it does not mean every part reaches equilibrium after the same number of hours.
ISO 1110 addresses accelerated conditioning of polyamides. Where it is used, the parties should agree on its applicability and confirm that the conditioned state is relevant to the intended evaluation. It should not automatically replace service-environment validation.
Pellet moisture determination is a separate task. ISO 15512 covers methods for determining water content in plastics. A suitable water-specific method, such as an applicable Karl Fischer procedure, can help distinguish moisture from other volatile substances. A loss-on-drying instrument may detect more than water, so its suitability and settings need validation for the resin concerned.
Stage One: Define the Service Condition and Critical Dimensions
Before choosing a material, identify whether the component will operate indoors, outdoors, near condensation, under intermittent splashing, or in continuous immersion. Record the expected temperature and humidity range rather than using “normal conditions” as the specification.
Consider an illustrative nylon sleeve assembled over a steel shaft. If the sleeve absorbs moisture, its bore, outer diameter, and interference conditions may change. The actual response depends on geometry, reinforcement, constraints, and moisture distribution. It is unsafe to infer the assembly result from a mass-absorption percentage alone.
Water absorption percentage is not a direct linear-expansion percentage. A reported mass gain cannot be applied to every drawing dimension as a scaling factor.
Identify dimensions that control function: bores, snap-fit engagement, sealing interfaces, locating features, and clearances around metal components. Validate those features in the relevant moisture states. Where moisture-related movement conflicts with the tolerance, options include a different grade, revised clearance, geometry changes, or a different assembly arrangement.
Glass reinforcement may improve dimensional stability in some directions, but it does not eliminate moisture sensitivity. Gate position and fiber orientation can influence the response of reinforced parts, making production-representative samples important.
Stage Two: Control Moisture Before and During Injection Molding
Plastic water absorption becomes a processing issue when moisture enters the melt. In hydrolysis-sensitive polymers, including many polyester and polycarbonate grades, water at processing temperature can break polymer chains. The resulting loss of molecular weight may reduce performance even when the surface looks acceptable.
Silver streaks, splay, bubbles, or unstable appearance can indicate moisture problems, but they can also arise from air entrapment, volatiles, or degradation. Appearance is a troubleshooting clue, not a moisture measurement.
Use the exact grade’s drying instructions
Drying temperature, time, airflow, dryer dew point, and maximum residual moisture should follow the resin supplier’s guidance. A generic “nylon drying setting” is not an adequate process specification for every PA grade, additive package, or initial moisture level.
Excess temperature or unnecessarily long drying can also damage some materials or additives. The target is verified processing readiness, not simply longer dryer residence.
- Keep material identification and packaging condition traceable at receipt.
- Follow supplier instructions for bringing sealed cold material into a warm production area.
- Check actual dryer operation and material throughput, not only controller setpoints.
- Use a validated moisture test with representative sampling where required.
- Limit moisture reabsorption during transfer, hopper residence, and interruptions.
- Control regrind storage, drying, and blend conditions where regrind is permitted.
A practical mistake is testing pellets at the dryer outlet while ignoring their condition at the machine feed. An open transfer container or extended production stop can undermine otherwise adequate drying. The control point should reflect the material that actually enters the process.
Stage Three: Approve Parts in a Defined Moisture State
A first-article report should state when parts were measured and how they were stored. Without that information, dimensional differences between factory inspection and incoming inspection can be difficult to interpret.
For moisture-sensitive components, an agreed validation plan may compare dry-as-molded parts, parts conditioned at a specified atmosphere, and parts exposed to a relevant service condition. These are distinct states and should be identified clearly in reports.
For example, a buyer evaluating a polyamide locating component could request measurements of critical features after defined post-molding handling and again after agreed conditioning. If immersion is part of actual use, a separate immersion evaluation may be necessary. These tests should not be combined into a single undefined “wet” condition.
Mass tracking can help establish moisture uptake, while dimensional inspection and functional assembly checks show its consequences. A stable mass alone does not prove that a tight-tolerance mechanism will work.
Do not correct the mold solely because dry and conditioned measurements differ. Establish whether the drawing applies to the dry state, the conditioned state, or both. Otherwise, a tooling correction that improves one inspection result may create a service-fit problem.
Packaging also needs a defined purpose. Moisture-barrier packaging can help preserve an agreed delivery condition, but it does not permanently prevent absorption after unpacking. Likewise, controlled post-molding conditioning may support assembly consistency, but it cannot reverse molecular damage caused by wet processing.
How Plastic Moisture Absorption Affects Cost and Lead Time
The commercial impact extends beyond resin price. A material with a lower purchase cost may require more drying control, longer conditioning, additional inspection, or different packaging to meet the same functional requirement.
Compare total manufacturing cost under a common acceptance basis. Relevant items include dryer energy, handling, moisture testing, conditioning space, inspection labor, packaging, and the risk of rejection after shipment. These costs depend on the actual grade, component geometry, production schedule, and agreed controls.
Conditioning can also become part of the delivery schedule. Thick sections may require more time than thin sections to approach a specified moisture state. If conditioned inspection is required, that time belongs in the project plan rather than being discovered after molding is complete.
At quotation stage, buyers should provide the drawing, exact material requirement or approved alternatives, service environment, critical tolerances, and acceptance condition. Any required moisture testing, conditioning, or special packaging should be included in the quotation scope.
Material substitutions deserve particular care. A change within the same polymer family can alter absorption, drying requirements, shrinkage, and dimensional response. Approval should cover the exact alternative grade and any necessary revalidation, not merely a matching generic material name.
Put Water Absorption Controls into the OEM Specification
For an injection-molded component, the most useful specification connects material identity, processing readiness, inspection condition, and service performance. A datasheet value alone cannot make those connections.
- Specify the approved resin manufacturer and grade, including reinforcement and relevant additives.
- Reference water-absorption data with its test method and exposure conditions.
- Identify the service environment and moisture-sensitive functional features.
- Define the moisture condition and timing for dimensional acceptance.
- Agree on grade-specific drying controls and moisture verification where necessary.
- Include conditioning, packaging, and inspection requirements in cost and lead-time discussions.
- Require review before material, regrind, packaging, or other relevant process changes.
For JATERSON’s general injection molding and hardware projects, the manufacturing priority is to align these requirements before sample approval and production ramp-up. This keeps material selection, tooling decisions, quality inspection, and delivery planning on the same basis.
Water absorption becomes manageable when it is treated as a defined project condition rather than an unexpected material defect. The goal is not always to choose the lowest-absorption plastic. It is to choose and validate a material that maintains the required function throughout molding, shipment, assembly, and use.


Recent Comments (0)0